Industries · Plastics
Dry Lubrication for Plastic Molding
Improve Mold Release. Reduce Cycle Times. Minimize Wear.
Dicronite® dry lubrication helps reduce friction on mold surfaces and moving components. Its ultrathin film supports precision tooling while helping address difficult demolding, part rejection, and maintenance requirements.
Reported applications include polypropylene closures, EVA seals, ejector pins, and sliding mold components.
- 25% Up to 25% shorter cycle time Reported for polypropylene undercut screw caps.
- <0.1% Reject rate, from about 1% Reported for polypropylene measuring cup closures.
- 1Mcycles Ejector pins, no noticeable wear 3 mm pins under a 70 N side load, in a reported test.
Why Dicronite®
Functional properties
-
Low friction
A reported coefficient of friction as low as 0.030 helps reduce sliding resistance. Performance depends on application conditions.
-
Precision film
A maximum thickness of 0.5 microns supports close-tolerance mold components with minimal dimensional buildup.
-
High-temperature stability
Reported temperature capability up to 538°C supports demanding tooling applications.
-
Versatile application
Suitable for evaluation on mold surfaces, ejector pins, slides, and other moving components.
Cycle times
Reduced molding cycle times
Reduced friction during demolding can help parts release more smoothly and shorten the molding cycle.
- Polypropylene undercut screw caps25%up to
- EVA seals15%reduction
- Polypropylene measuring cup closures10%reduction
- Force-demolded polypropylene notched snaps12%plus fewer rejects
Part quality
Fewer rejected parts
Smoother release can help reduce jolting and damage during force-demolding.
In a reported polypropylene measuring cup closure application, the reject rate decreased from approximately 1% to below 0.1% following reduced jolting during demolding.
A separate polypropylene notched snap application reported fewer rejects alongside a 12% reduction in cycle time.
Reject rate · measuring cup closures
Following reduced jolting during demolding.
Wear and maintenance
Reduced wear and maintenance costs
Ejector pins
Ejector pin performance
1McyclesA reported test involving 3 mm ejector pins under a 70 N side load reached one million cycles with no noticeable wear.
Sliding components
Sliding component cost savings
10:1Sliding components used to form the internal honeycomb contour of molded polyamide gear levers delivered a reported 10:1 ratio of cost reduction to Dicronite application cost.
Filling pressure
Potential for lower filling pressure
In molds with long flow paths and thin walls, reduced surface friction may help lower the required filling pressure.
Where achieved, lower filling pressure may help reduce flash, decrease energy costs, and extend mold service life.
Contact Dicronite Southwest
Discuss your plastic molding application
Contact Dicronite Southwest to discuss mold release challenges, component wear, tooling tolerances, and opportunities to improve your molding process.
The figures above describe specific reported applications and tests. Results depend on resin, tooling geometry, processing conditions, and component loading.